Nickel - based alloys find extensive application in aerospace, chemical, marine engineering, and nuclear sectors, all thanks to their outstanding performance when exposed to high temperatures and highly corrosive surroundings. Inconel 625 and Inconel 718 stand out as two typical high - performance alloys within this category. Despite sharing membership in the Inconel family and boasting commendable oxidation and corrosion resistance, they differ greatly in terms of their composition, mechanical characteristics, heat treatment approaches, and practical uses. Gaining an understanding of how Inconel 625 and 718 (Inconel 625 vs 718) vary is of great significance for material selection and engineering design. In the following sections, we will examine the similarities and differences between these two alloys from the perspectives of their composition, performance comparison, and typical applications. For any inquiries, please get in touch with C&N.
AISI Alloy 625 Alloy 686 Stud Full Thread Uns N06625 N06686 Inconel Alloy Steel

AISI Alloy 625 Alloy 686 Stud Full Thread Uns N06625 N06686 Inconel Alloy Steel

Equivalent Grades

STANDARD WERKSTOFF NR. UNS GOST AFNOR JIS BS EN OR
Inconel 625 2.4856 N06625 ХН75МБТЮ NC22DNB4M NCF 625 NA 21 NiCr22Mo9Nb ЭИ602
Inconel 718 2.4668 N07718

Chemical Composition

Grade Ni Fe C Mn Si Cr2 Mo Co Al Ti Nb + Ta P S
Inconel 625 58.0 min 5.0 max 0.10 max 0.50 max 0.50 max 20.0-23.0 8.0-10.0 1.0 max 0.40 max 0.40 max 3.15–4.15 0.015 max 0.015 max

 

Grade C Mn Si S Cu Fe Ni Cr
Inconel 718 0.08 max 0.35 max 0.35 max 0.015 max 0.30 max - 50.00 - 55.00 17.00 - 21.00

Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 625 8.4 g/cm3 1350 °C (2460 °F) Psi - 1,35,000 , MPa -930 Psi - 75,000 , MPa - 517 42.50%
Inconel 718 8.2 g/cm3 1350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 482 45%

What is Inconel 625?

Inconel 625, also referred to as Incoloy 625, is an alloy primarily made up of nickel, chromium, and molybdenum. It demonstrates exceptional resistance to pitting and corrosion cracking. This alloy maintains remarkable mechanical properties across a wide temperature range, from extremely low to high temperatures. It possesses high fracture strength and tensile strength, along with excellent weldability and brazing capabilities. Inconel 625 shows great resistance to corrosion caused by inorganic acids like sulfuric acid, hydrochloric acid, phosphoric acid, and nitric acid. The high nickel content in the alloy allows it to endure harsh corrosive environments such as neutral salts, alkaline media, and seawater.

What is Inconel 718?

Inconel 718 is a nickel - based high - temperature alloy, with its main components being nickel, chromium, iron, and titanium. It has excellent oxidation resistance and can keep its mechanical properties stable at high temperatures. For this reason, it is widely used in the production of components that operate in high - temperature environments.
Another feature of this alloy is that its structure is extremely sensitive to thermal processing techniques. It is crucial to grasp the laws governing the precipitation and dissolution of alloy phases, as well as the interrelationships between the structure and process performance. By formulating reasonable and feasible process procedures based on different usage requirements, a variety of parts that meet different strength levels and usage needs can be obtained.

Corrosion resistance

Inconel 625:

Due to its high content of chromium, molybdenum, and niobium, Inconel 625 displays excellent corrosion resistance in a wide range of extreme environments, particularly in oxidizing and reducing conditions. It performs well in brine, seawater, acidic media, and high - temperature chloride and sulfate environments. As a result, it is commonly utilized in the chemical, marine engineering, nuclear, and aerospace industries.

Inconel 718:

Although Inconel 718 is not as corrosion - resistant as Inconel 625, it still has good corrosion resistance under high - temperature and high - pressure conditions, especially in high - temperature oxidation and creep environments. This makes it an ideal material for manufacturing aero - engine turbine components, rocket engine parts, and nuclear reactor components.

Thermal Processing

Inconel 625 has good thermal processing properties and a wide range of thermal processing temperatures, usually between 950 - 1200℃. During the hot working process, it is important to control the heating rate and deformation to prevent defects such as overheating and overburning.
Inconel 718 is relatively difficult to hot work because of its high alloying degree. The hot working temperature must be strictly controlled within 950 - 1050℃. Within this temperature range, the alloy has good plasticity, which can effectively avoid the occurrence of thermal cracks. At the same time, the cooling rate after hot working also has a significant impact on the structure and properties of the alloy.

Cold working

Inconel 625 has good cold working performance and can undergo processing operations such as stamping and cold forming. However, during the cold working process, as the processing deformation increases, the material will experience work hardening. Therefore, timely intermediate annealing treatment is necessary to restore the plasticity of the material.
Inconel 718 is also prone to work hardening during cold working, and due to its high strength, there are more stringent requirements for processing equipment and molds. Usually, a combination of multiple cold working and intermediate annealing processes is required. The intermediate annealing temperature is generally around 850℃ to reduce the hardness of the material and improve its processing performance.

Weldability

Inconel 625 has excellent weldability and is relatively resistant to post - weld cracking. This makes it easier to handle when fabricating complex structures and reduces the risk of weld defects.
Inconel 718 also has excellent weldability and a high resistance to post - weld (age) cracking, which is a significant advantage among precipitation - strengthened alloys. However, due to its complex strengthening mechanism, welding parameters and processes need to be strictly controlled during welding to ensure that the mechanical properties of the final part are not affected. Improper welding can lead to a decline in performance or cracking in the weld area.

Strength

Inconel 625 has good and consistent strength in the annealed state. This is an advantage for applications that do not require extremely high strength or where a simplified manufacturing process is preferred. However, its strength level is generally not as high as that of age - hardened Inconel 718.
When properly age - hardened, Inconel 718 can exhibit very high yield, tensile, and creep fracture strengths. This is a key reason for its popularity in high - stress, high - temperature applications such as aerospace and gas turbines. Its strength advantages are particularly prominent within specific temperature ranges.
UNS N06625 Inconel 625Hex Bolts PMI test

UNS N06625 Inconel 625Hex Bolts PMI test

Inconel 625 Advantages:

  1. Excellent corrosion resistance: It performs well in various harsh corrosive environments, especially in seawater, acidic media, and chloride environments.
  2. Good high - temperature strength: It has high mechanical properties and oxidation resistance at elevated temperatures.
  3. Excellent fatigue strength and resistance to stress corrosion cracking.
  4. No need for age - hardening: Good strength can be achieved in the annealed state, simplifying the manufacturing process.
  5. Good weldability and formability.

Inconel 625 Disadvantages:

  1. Its strength is not as high as that of age - hardened Inconel 718.
  2. Higher cost.
  3. More difficult to machine.

Inconel 718 Advantages:

  1. Very high strength: After age - hardening, it has excellent tensile, yield, creep, and fracture strength over a wide temperature range (from cryogenic to 700℃).
  2. Excellent fatigue resistance.
  3. Good weldability: High resistance to post - weld cracking, which is essential for the manufacture of complex components.
  4. Good oxidation resistance at high temperatures.

Inconel 718 Disadvantages:

  1. Its corrosion resistance may be slightly lower than that of Inconel 625 in some extreme environments.
  2. It requires complex age - hardening heat treatments to achieve optimal performance.
  3. High cost.
  4. Difficult to machine and tends to work - harden.

Conclusion

Inconel 625 and Inconel 718 are two important nickel - based superalloys, each with unique performance advantages and application scenarios. Inconel 625 excels in corrosion resistance and is suitable for fields such as oil and gas and chemical industry that require high corrosion resistance. Inconel 718 has advantages in high - temperature strength, fatigue performance, and hardness, and is mainly used in aerospace, high - performance automobile engines, and other fields with strict requirements on the mechanical properties of materials. In actual engineering applications, engineers and manufacturers should select appropriate alloys based on specific usage environments, performance requirements, processing technologies, and costs to ensure that the quality and performance of products are optimized.